No Detail Found!

Integrated technologies for desulfurization of cryptocrystalline graphite

Author(s)
Gilmanshina T. R. Department of Engineering Baccalaureate CDIO, Institute of Non-Ferrous Metals and Materials Science, Siberian Federal University,Krasnoyarsk,Russia
Koroleva G. A. Department of Fundamental Natural Science Education, Institute of Non-Ferrous Metals and Materials Science, Siberian Federal University,Krasnoyarsk,Russia
Dubova I. V. Department of Fundamental Natural Science Education, Institute of Non-Ferrous Metals and Materials Science, Siberian Federal University,Krasnoyarsk,Russia
Vasyunina N. V. Department of Nonferrous Metals Metallurgy, Institute of Non-Ferrous Metals and Materials Science, Siberian Federal University,Krasnoyarsk,Russia
Lytkina S. I. Department of Materials Science and Materials Processing Technologies, Polytechnic Institute, Siberian Federal University,Krasnoyarsk,Russia
Masanskii O. A. Department of Materials Science and Materials Processing Technologies, Polytechnic Institute, Siberian Federal University,Krasnoyarsk,Russia
Khudonogov S. A. Department of Applied Mechanics, Polytechnic Institute, Siberian Federal University,Krasnoyarsk,Russia
Berezyuk V. G. Department of Materials Science and Materials Processing Technologies, Polytechnic Institute, Siberian Federal University,Krasnoyarsk,Russia
Vonog V. V. Department of Foreign Languages for Engineering, Siberian Federal University,Krasnoyarsk,Russia
Abstract
An increase in the carbon content in cast iron and steel during smelting is carried out by adding carbon-containing materials to the charge - carburizers (carburetors). For the fastest and most complete assimilation of carbon, the carburetor must have a minimum amount of impurities and a low ash content. As the ash content of the carburizer decreases, the amount of slag also decreases, which in turn increases the durability of the furnace lining. To prevent the cast iron from becoming unnecessarily saturated with sulfur, the carburetor must contain a minimum amount of sulfur. Currently, coals and natural graphites are widely used as carburetors. Compared to other carbon-containing materials, natural graphites are of limited use because of the high sulfur content, which is represented by pyrite (polysulfide form) or is in the sulfide form in the form of disseminations and aggregative accumulations 2 × 1 mm in size. Therefore, the aim of the work is to develop graphite desulfurization technologies that allow reducing the sulfur content to 0.05%. In this work, mechanical activa tion, electroexplosive impulse activation, and oxidative leaching were used to desulphurize graphite. It is shown that each of the proposed methods intensifies all subsequent processes of sulfur extraction from graphite, more fully disclosing it from pyrite, pyrrhotite and chalcopyrite particles. Various combinations of these methods make it possible to obtain graphite of the required purity. Processing of graphite according to schemes, including electroexplosive-pulse processing followed by oxidative leaching and mechanical activation, followed by electroexplosive-pulse processing and oxidative leaching, makes it possible to reduce the sulfur content 1 to 0.16-0.21%. At the same time, the use of a combined scheme, including mechanical activation and oxidative leaching, reduces the sulfur content in the composition of graphite to 0.06-0.09%, replacing the oxidative leaching operation with steam treatment of graphite, to 0.05%.
Publication Details
Page(s) 416-423
DOI DOI not available
Published Journal: ARPN Journal of Engineering and Applied Sciences, Volume: 17, Issue: 4, Year: 2022

Request the full text from PASTIC

Keywords
mechanical activation, oxidative leaching, Desulfurization, electro-explosive impulse activation, cryptocrystalline graphite
References
Murakami T.,Ohno M.,Suzuki K.,Owaki K.,Kasai E. .2017 .Acceleration of carburization and melting of reduced iron in iron ore-carbon composite using different types of carbonaceous materials. ISIJ International, 57(11) : 1928-1936.
Stercken K.,Bandusch L. .1978 .Different carburising agents in the EAF production of high-carbon steel grades. MPT Metallurgical Plant and Technology International, 22(4) : 5.
Chapman M. W.,Monaghan B. J.,Nightingale S. A.,Mathieson J. G.,Nightingale R. J. .2007 .Observations of the mineral matter material present at the coke/iron interface during coke dissolution into iron. ISIJ International, 47(7) : 973-981.
Montillo I. A.,Montillo L. I. Kiseleva,Nikitin Yu. A. .1978 .Non-ferrous metals. , : 23-25.
0

Citations

0

Downloads

8

Views