Consistency, setting time and compressive strength of cement blended with marble rock powder.

Author(s)
Bazid Khan Department of Civil Engineering, CECOS University of IT and Emerging Sciences, Hayatabad, Peshawar, Pakistan
Abdul Khaliq Kurd Department of Civil Engineering, Balochistan University of Engineering and Technology, Khuzdar, Pakistan
Abstract
This research studies the potential of using MRP (Marble Rock Powder) as a blended cement material. The powder was used to replace ASTM Type-I, OPC (Ordinary Portland Cement) in pastes and mortars. The levels of replacement of cement by an equal amount of the powder were 5, 10, 20, 25, and 30% by weight. A reference cement paste and mortar were also prepared for comparison. The blends were tested for their normal consistency, initial and final setting times, and compressive strengths. The results were compared to those of reference paste and mortar. A Vicat apparatus was used for checking normal consistency and setting times. Cubes of 5cm were tested for compressive strengths. The strength tests were done after 1, 3,7,14, and 28 days. Results of the experimental study indicate that water demand for normal consistency of the blends was continuously increasing with increasing level of cement replacement by the powder; however, the change is not of greater range. The normal consistency for reference paste is 27.33% by weight of binder (cement+powder) while it raised to 30.33% for paste with 30% replacement level of OPC by MRP. There is no considerable change in both initial and final setting times of the blended pastes up to 15% replacement level; however, for pastes with 20% and higher replacement level, the setting times dropped below the setting times of the reference paste. In comparison to setting time of the reference paste, the initial and final setting times of pastes having higher MRP content were shortened by 57 (19.2%) and 54 (16.6%) minutes respectively. Mortars with 5, 10 and 15% replacement level showed higher compressive strength at all ages than the reference mortar. The 28-days strengths for reference mortar is 14.20 N/mm2 while for mortars with 5,10 and 15% replacement level, the strengths are 15.95, 15.05 and 14.79 N/mm2 respectively. The mortars with 20, 25 and 30% replacement level showed lower strengths after one day; however, their later strengths are comparable with that of the reference mortar.
Publication Details
Page(s) 405-416
DOI DOI not available
Published Journal: Mehran University Research Journal of Engineering and Technology, Volume: 29, Issue: 3, Year: 2010