Localized corrosion study of 316L bio-implant in simulated body fluids

Author(s)
H. Khurshid Department of Metallurgy & materials Engineering, CEET, University of the Punjab, 54500, Lahore, Pakistan
K. M. Deen Department of Metallurgy & materials Engineering, CEET, University of the Punjab, 54500, Lahore, Pakistan
S. L. Ahmad 26 E Main Market, Gulberg-II, 54000, Lahore, Pakistan
R. Ahmad Department of Metallurgy & materials Engineering, CEET, University of the Punjab, 54500, Lahore, Pakistan
Abstract
This study was to investigate the behavior of corrosion resistance of 316L austentic stainless stainless steel bio-implant. The localized corrosion behavior of 316L in simulated body fluids (ringer, ringer+0.1% blood serum. Ringer + 0.4% blood serum and 1% lactic acid solution) was investigated by electrochemical cyclic polarization test method. It was deducted by electrochemical test results that pitting resistance of 316L SS increased with the addition of blood serum in ringer solution. Formation of meat stable pits was evident from polarization curves with the addition of blood serum. The addition of lactic acid further reduced the stable pitting tendency of 316L SS.
Publication Details
Page(s) 275-278
DOI DOI not available
Published Journal: Science International, Volume: 23, Issue: 4, Year: 2011