No Detail Found!

Failure of Crude Oil Heater Tubes

Author(s)
K. M. Deen Faculty of Engineering & Emerging Technology, University of the Punjab, 54590 Lahore, Pakistan
I. H. Khan Faculty of Engineering & Emerging Technology, University of the Punjab, 54590 Lahore, Pakistan
M. A. Virk Technical Services Centre, Pakistan Standard and Quality Control Authority, 54000 Lahore, Pakistan
K. M. Ghauri Department of Metallurgical and Materials Engineering, University of Engineering & Technology, 54890, Lahore, Pakistan
Abstract
The “Up-country oil refinery”approached for the investigation of frequent failures of crude heater tubes due to corrosion. The failed tubes were characterized by visual observation, chemical analysis of material, and microstructurally. The crude oil physical and chemical characteristics were also determined. It was confirmed that the material of failed crude heater tube was within the specification as per design.It was inferred from the obtained data that the heating furnace was operating efficiently for the feed oil from source 1. It was evident from the investigation that the failure of heater tubes became frequent when the crude oil feed was switched to source 2 from source 1. The careful in-depth study revealed that higher H2S content in the crude from source 2 (11-23ppm) caused severe corrosion damage of heater tubes in the radiation zone made of carbon steel designed originally based on source 1 crude oil.
Publication Details
Page(s) 89-93
DOI DOI not available
Published Journal: Journal of Pakistan Institute of Chemical Engineers, Volume: 39, Issue: 1, Year: 2011

Request the full text from PASTIC

0

Citations

0

Downloads

43