No Detail Found!

Characterization of As-Deformed microstructure of ODS Ni-Base superalloy and ODS ferritic steel prior to directional recrystallisation.

Author(s)
Muhammad Moazzam Baloch Department of Metallurgy & Materials Engineering, Mehran University of Engineering & Technology, Jamshoro, Pakistan
Sikandar Ali Memon Department of Metallurgy & Materials Engineering, Mehran University of Engineering & Technology, Jamshoro, Pakistan
Abstract
The materials studied are unusual in the sense that they have been prepared from mechanically alloyed procedures, including compaction and “hot” extrusion. It was felt necessary to characterize the initial microstructure thoroughly prior to directional recrystallisation of the alloys. Following consolidation by hot extrusion, dispersion strengthened superalloys appear to display a very fine sub-micron grain size consisting of both dislocation free recrystallised material and un-recrystallised regions of high dislocation density. It is found that there is a very fine dislocation cell structure in the ODS (Oxide Dispersion Strengthened) Ferritic Stainless Steel prior to recrystallisation treatment, which shows that alloy is in cold-deformed condition after mechanical alloying, extrusion / hot working. This is in contrast to the mechanically alloyed Nickel Based Superalloy, which have consistently been found to be in primary recrystallisation state following extrusion. In order to understand the recrystallisation behavior of the two mechanically alloyed materials with commercial designations MA 6000 and MA 956, a measurement of the orientation relationship between adjacent grains in the as-deformed ODS alloys has also been carried out using Transmission Electron Microscope.
Publication Details
Page(s) 345-354
DOI DOI not available
Published Journal: Mehran University Research Journal of Engineering and Technology, Volume: 26, Issue: 4, Year: 2007

Request the full text from PASTIC

0

Citations

0

Downloads

25

Views