No Detail Found!

Metallurgical analysis of high pressure gas pipelines rupture.

Author(s)
F. Hasan Department of Metallurgical and Materials Engineering, University of Engineering and Technology, Lahore, Pakistan
F. Ahmed Department of Metallurgical and Materials Engineering, University of Engineering and Technology, Lahore, Pakistan
Abstract
On 6th July 2004, two parallel-running gas pipelines (18-inch and 24-inch) diameters), in the main transmission network of SNGPL (a gas company in Pakistan) were ruptured. The ruptures occurred in the early hours of the morning about 8 miles downstream of the compressor station AC-4. The ruptures were indicated by the increased gas flow at the outlet of AC-4, first at about 0648 hours and then again about 20 minutes later. The gas escaping from the ruptured lines has caught fire, and the flames had also ‘affected’ a third parallel-running pipeline of 30-inch diameter, lying next to the 24-inch line. The metallurgical examination of the two ruptured lines showed that the 24-inch line was ruptured with the help of an explosive device that had been placed on the underside of the pipe. An examination of the 18-inch line showed that this pipe had failed as a result of the heating of the pipe-wall, presumably, by the flame emanating from the 24-inch line. These two observations clearly suggested that the 24-inch line was the first to rupture (by explosives), and the fire following this rupture had heated the 18-inch pipe to a temperature where its yield strength was unable to support the inside gas pressure. The 20 minutes time interval between the two ruptures was obviously the time taken by the 18-inch pipe to be heated up to the level where it started to yield. The 30-inch line lying next to the 24-inch line was affected to the extent that its coating had been burnt-off over a length about 40-50 feet. However, the pipe did not exhibit any sings of de-shaping or deformation what-so-ever. A replica metallographic examination indicated that the microstructure of the pipe was not measurably affected by the heat. It was thus decided not to replace the “affected “part of the 30-inch pipe, but only to re-coat this affected portion.
Publication Details
Page(s) 14-23
DOI DOI not available
Published Journal: Pakistan Journal of Engineering and Applied Sciences, Volume: 1, Issue: , Year: 2007

Request the full text from PASTIC

0

Citations

0

Downloads

43

Views