The corrosion behavior of pure tin in de-aerated solutions of oxalic, tartaric and citric acids in the presence and absence of NO2, NO3 and CI- anions were studied by means of potential-time measurements, corrosion rate and galvanostatic technique at the pH range 2.5 -6.5 for O.1 M of the three tested acids. At pH 4.5 there is a maximum negative potential for oxalic acid and at pH 5.5 for tartaric and citric acids. From pH 2.5 to 4.5, the corrosion mechanism is anodically controlled by the reaction of Sn+2ion with the anion of the tested acids. At pH 5.5 the corrosion of tin is reduced which may be due to the formation of a film on the tin electrode resulting from the hydrolysis of tin complex species. The potential of the tin electrode in the three tested acidic solution tends to be shifted to the less negative values in the presence of additives NO2, NO3 and CI anions at pH4.5.