Reduction of indigenous antimony ore (stibnite) to antimony metal without using iron.

Author(s)
M. I. Bhatti Pakistan Council of Scientific and Industrial Research (PCSIR) Laboratories, Lahore, Pakistan
Kalim Akhtar Pakistan Council of Scientific and Industrial Research (PCSIR) Laboratories, Lahore, Pakistan
Abdul-Hamid Pakistan Council of Scientific and Industrial Research (PCSIR) Laboratories, Lahore, Pakistan
Khalid Masood Pakistan Council of Scientific and Industrial Research (PCSIR) Laboratories, Lahore, Pakistan
Abstract
An attempt has been made to extract antimony metal from indigenous (Chitral), antimony ore (Stibnite), without using iron which is used in usual Iron Precipitation Method. The method involves direct reduction of antimony sulphide present in the ore with soda ash and carbon-bearing reducing agent such as wood charcoal. Optimum conditions with respect to the amounts of different components of the charge, temperature of reduction and duration of operation were established. The appropriate amounts of different components of the charge containing 500 gms of stibnite (28.5% Sb2S3) were found to be 200-270 gms of soda, 50-60 gms of charcoal, smelting temperature 900-950C and holding time at this tern. 1-1/2 - 2 hours. The maximum output under these conditions of smelting amounted to 93-95% antimony with a purity of 99-99.2%.
Publication Details
Page(s) 13-17
DOI DOI not available
Published Journal: Pakistan journal of scientific research, Volume: 41-42, Issue: , Year: 1989