N-vinylcarbazole-divinylbenzene copolymers, Formation of porous structure by using cyclohexanone and petroleum ether as diluents in suspension polymerization.

Author(s)
Muhammad Abdul Hamid Applied Chemistry Division, Pakistan Institute Nuclear Science & Technology (PINSTECH), Islamabad, Pakistan
Riffat Naheed Applied Chemistry Division, Pakistan Institute Nuclear Science & Technology (PINSTECH), Islamabad, Pakistan
Ejaz-Ur-Rehman Applied Chemistry Division, Pakistan Institute Nuclear Science & Technology (PINSTECH), Islamabad, Pakistan
Abstract
A number of copolymers were synthesized by the reaction of N-vinylcarbazole (NVC) and divinylbenzene (DVB) by using the technique of suspension polymerization. A mixture of cyclohexanone (CHN) and petroleum ether (pet.ether) of various compositions was used as a diluents in the polymerization experiments. The copolymers were characterized for the apparent density, pore volume, pore size distribution, surface area and mechanical strength. The copolymers were also converted into cation-exchange resin by sulfonation and the resulting resins were characterized for their ion-exchange capacity. The pore volume of the copolymers decreases from 1.26 to 0.19 ml/g and 1.09 to 0.46 mVg with the decrease in pet. ether or increase in CHN ratio of organic phase, with the decrease in the amount of diluents as compared to monomers (Fs) and with the decrease in the cross linking agent, DVB respectively, used in the respective polymerization experiments. The apparent density of the copolymers varies from 0.55 to 0.25 m/ml, 0.55 to 0.27 m/ml and 0.45 to 0.28 g/ml with the percentage increase in the ratio of pet. Ether from 0. to 100% as compared to CHN, with the increase in solvent fraction from 0.3 to 0.8 and with the increase in DVB from 5 to 40% respectively. The relatively larger size pores were observed in the beads of copolymers formed with the increase in the pet, ether contents of the diluents, increase in the amount of diluents as compared to monomers and also with the increase in the cross linking agent. The capacity of NVC-DVB cation-exchange resins decreased slightly from 4.89 to 4.00 meq/g with the increase in the cross linking agent from 5 to 40% whereas it does not change significantly with change in the composition and the amount of diluents used in polymerization experiments under the given experiment conditions. The surface area decreases from 89 to 10 m2/g , 133 to 1 m2/g and 237 to 14 m2/g with the decrease in pet, ether or increase in CHN's ratio in diluents mixture, decrease in the solvent fraction (Fs) and decrease in the cross linking agent under the given experimental conditions. The mechanical strength (crushing load) of the copolymer beads increases with the increase in CHN ratio from 0 to 100% in diluents mixture with the decrease in colvent traction from 0.8 to 0.3 and with it decrease in the cross linking agent (DVB) from 40 to 5%. The crushing load also increases with the increase in the overall size of the polymer beads.
Publication Details
Page(s) 119-127
DOI DOI not available
Published Journal: Nucleus, Volume: 33, Issue: 4, Year: 1996

Request the full text from PASTIC