Macro porous glycidyl methacrylate/ethyleneglycol dimethacrylate and styrene/divinylbenzene copolymers- a comparison.

Author(s)
Munir Ahmed Applied Chemistry Division, Pakistan Institute Nuclear Science & Technology (PINSTECH), Islamabad, Pakistan
Muhammad Arif Malik Applied Chemistry Division, Pakistan Institute Nuclear Science & Technology (PINSTECH), Islamabad, Pakistan
Abstract
Macro porous beads of copolymers of glycidyl methacrylate/ ethyleneglycol dimethacrylate (GDM-EGD) and of styrene/divinlylbenzene (St-DVB) are synthesized in the presence of different diluents. The GDM-EGD copolymers of pore volume around 0.05-I ml/g and St-DVB copolymers of pore volume around 0.05-0.4 ml/g are synthesized by employing mixture of cyclohexanone (CHN) and petroleum ether (PE) with CHN:PE ratio varying from 100.0 to 0.100. The St-DVB copolymers are converted into cation exchangers through suffocation with H2SO4. Highest pore area along with good crush strength and ion exchange capacity is observed when pore volume is 0.4-0.5 ml/g. For GDM-EGD copolymers this pore volume is achieved at CHN:PE ratio of 85:15-67:33 and for St-DVB copolymers at 0:100.
Publication Details
Page(s) 133-137
DOI DOI not available
Published Journal: Nucleus, Volume: 44, Issue: 4, Year: 1996