Some studies on thermo-oxidative degradation of polyester fiber.

Author(s)
M. S. Rizvi Applied Chemistry Department, University of Karachi, Karachi, Pakistan
Abstract
Effect of heat on Polyester Yarn produced from poly (ethylene terephthalate) in the normal atmosphere, that is air containing small amount of moisture, has been studied. Tenacity of Polyester Yarn has been measured at temperatures upto 200 C°. From these measurements, it is concluded that Tensile strength varies inversely with temperature. Exposed to a temperature of 150 C° for 72 hours, the yarn loses only 7.196 of its original strength. While loss is only about 28.8% at 180 C°, and exposed to 200 C° for the same period it loses 41.1% of its original strength. The darkening in color is small even at temperatures in the region of 180 C°.
Publication Details
Page(s) 1-4
DOI DOI not available
Published Journal: Karachi University Journal of Science, Volume: 11, Issue: 1, Year: 1983

Request the full text from PASTIC

0

Citations

0

Downloads

26

Views