Molecular weight of unfractionated cellulose acetate was determined by turbidity measurements, using light scattering photometer for 436nm and 546nm wave-lengths at 25°C. For comparison, the molecular weight of cellulose acetate was determined by Zimm plot method at the same wave-lengths and at the same temperature. It is concluded, that the values obtained by the two methods are in good agreement with each other. The determination of particle size of cellulose acetate was carried out, by the dissymmetry measurements, using wavelengths of 436nm at 25 °. The values of diameter and radius of gyration were calculated. These are well within the range of literature.