Direct potentiometric titration of walnut shells charcoal were made with aqueous sodium hydroxide, alcoholic potassium hydroxide and sodium ethoxide, potassium isopropoxide in isopropanol and potassium tert-butoxide in tert-butanol as the titrants. The titration curves of demineralized samples with aqueous sodium hydroxide showed inflection corresponding to the titration curve of CO2 and were in no way comparable in strength to carboxylic acids. Titration curves of variously treated charcoal samples with alcoholic potassium hydroxide, sodium ethoxide, potassium iso-propoxide and potassium tert- butoxide showed breaks, which were however not sharp enough to be ascribed confidently to definite surface acidic groups. The approximate total acidity of variously treated charcoal samples measured with potassium tert-butoxide, the strongest of the bases, is the lowest. Which indicates the profound negative effect due to bulky sizes of the bases on the extent of neutralization. These bulky sized bases get access with difficulty into the micropores in the charcoal structure to react with the acidic sites within the short interval of time i.e. 2-3 minutes which were required for the apparent stabilization of pH or mV.