No Detail Found!

Investigation of phases developed in bi4ti3o12 system by thermal and analytical techniques.

Author(s)
S. NAZ Microstructral Studies Group, Physics Division, Directorate of Science, Pakistan Institute of Nuclear Science and Technology, Islamabad, PAKISTAN
M. SHAHZAD Microstructral Studies Group, Physics Division, Directorate of Science, Pakistan Institute of Nuclear Science and Technology, Islamabad, PAKISTAN
A. QURESHI Microstructral Studies Group, Physics Division, Directorate of Science, Pakistan Institute of Nuclear Science and Technology, Islamabad, PAKISTAN
H. N. WAQAS Microstructral Studies Group, Physics Division, Directorate of Science, Pakistan Institute of Nuclear Science and Technology, Islamabad, PAKISTAN
H. HUSSAIN Microstructral Studies Group, Physics Division, Directorate of Science, Pakistan Institute of Nuclear Science and Technology, Islamabad, PAKISTAN
K. SAEED Microstructral Studies Group, Physics Division, Directorate of Science, Pakistan Institute of Nuclear Science and Technology, Islamabad, PAKISTAN
L. ALI Department of Metallurgical & Material Engineering, University of Engineering & Technology (UET), Lahore, PAKISTAN
Abstract
Bismuth titanate (Bi4Ti3O12) powders were prepared by conventional mixed oxide method using oxide mixture i.e. bismuth oxide (Bi2O3) and titanium oxide (TiO3). The mixed powders were ball milled for different times (8, 16, and 24h). The phase formation was investigated by X-ray diffraction (XRD) and results revealed that milled powder was mainly consisted of phases Bi2O3, TiO2 and small amount corresponded to Bi4Ti3O12. However, after calcination at 700ºC, Bi4Ti3O12 phase was mainly observed. Thermal decomposition behavior (DSC-TGA-DTA) was investigated as a function of milling time. Thermal analysis alongwith XRD results showed that the formation of desire phase (Bi4Ti3O12) was only possible above 600ºC. Single phase Bi4Ti3O12 ceramic was obtained with the orthorhombic structure by sintering at 800ºC. Maximum density (8.61g/cm3) was achieved in sample milled for 24h due to reduction in particle size which ultimately enhanced the diffusion process during sintering.
Publication Details
Page(s) 101-106
DOI DOI not available
Published Journal: Nucleus, Volume: 48, Issue: 2, Year: 2011

Request the full text from PASTIC

0

Citations

0

Downloads

95

Views