A successful attempt has been made to manufacture barium carbonate from indigenous barite by a process involving reaction between barite and an aqueous solution of soda ash under atmospheric pressure. The effects of such variables as particle size, temperature, time and concentrations of the reactants on the reaction yield were studied, Highest conversion obtained was 95.80%.