Preparation of aluminum sulphate from beneficiated Bijaipur clay (uncalcined and calcined) by sulphuric acid treatment has been studied. Optimum conditions for maximum yield of aluminum sulphate in solution have been determined with respect to calcination time and temperature, leaching time, concentration and volume of acid used for leaching. The maximum alumina extracted as aluminum sulphate has been found to be about 84.5% of the total alumina content of the calcined clay.