C2C114 has been found more effective for selective chlorination of iron constituent in chromite. At 750oCin four hours 68.7% of iron was chlorinated, while conversion of Cr2O3 was only 2.4%. The Cr/Fe ratio in the residue was 8.78. A pretreatment of the chromite in air with a mixture of NaC1 at 8500 improves the extent of conversion of iron to 87.2% but simultaneously considerable (23. 7%) amount of Cr2O3 is also effected.