No Detail Found!

Influence of different preparation conditions on catalytic activity of AG /?-AL2O3for hydrogenation of coal slime Pyrolysis.

Author(s)
Zhang Lei School of Geology and Environment, Xi’an University of Science and Technology, Xi’an, China
Shu Xin-Qian School of Chemical and Environmental Engineering, China University of Mining & Technology, Beijing, China
Zhang Lei Environmental Protection and Energy-Saving Equipment Research institute, China National Heavy Machinery Research Institute co, Ltd, Xi’an, 710032, China
Chen Rong School of Geology and Environment, Xi’an University of Science and Technology, Xi’an, China
Abstract
This paper, introducing variable conditional factors with Ag/AL2O3 as catalyst, selects five variables to investigate the influences of experimental conditions on Ag/Al2 O3 catalytic activity and define the optimal process conditions. These variables include Ag loading amount, calcinations temperature, calcinations time, reduction temperature, reduction time. X ray diffraction (XRD), hydrogen temperature-programmed reduction (TPR), X ray photoelectron spectrum (XPS) and scanning electron microscopy (SEM) were utilized to characterize the catalytic activity of Ag/γ-Al2O3, active center structure and state and those of carrier were emphatically studied, In the meantime the effects of active center and carrier on catalytic activity are studied. The results showed that: (1) In the range of 600 oC~900oC, the catalytic activity of Ag/γ-Al2O3 with different loading showed little difference when changing loading amount, in the range of 900 oC~1100oC, when the loading was 5%, the catalytic activity was very high; From the XRD and SEM characterizations, when the loading was 5%, it showed strong intensity diffraction peak of Ag crystal, crystal Ag is the most important activity center to promote hydrogen yield. (2) the catalytic activity of Ag/γ-Al2O3 at 450oC was considerably higher than that at 400oC and 500oC. By BET, XRD and SEM characterization, it can be seen, the diffraction peaks intensity of Ag crystal at 450oC is higher and sharper than that at 400oC and 500oC and with the increase of calcinations temperature, the specific surface area of catalysts also increased. (3) In the range of 600oC ~ 1000oC, the effects of calcinations time can be negligible, while, with temperature higher than 1000.C, 4-hour-calcinations-time catalyst exhibits a more noticeable catalytic activity than 3-hour and 5-hour catalyst do; From the XRD spectrogram, we can see that three kinds of catalysts all showed diffraction peaks of Ag and the diffraction peaks intensity of elemental Ag of the catalysts prepared at the calcination time of 4hour was higher and sharper than that prepared at 3hou and 5hour. (4) When reduction temperature was 450oC, the catalyst showed excellent activity, the catalytic activity of Ag/γ-Al2O3 was decreased after 1000oC when the reduction temperature at 400oC and 500 oC; (5) The reduction time had very little influence on the catalytic activity of catalyst. In the range of 600~1100oC, the catalytic activity of reduction time of 3 hour and 4 hour was the most significant, and when reduction time was 5 hour, the catalytic activity significantly reduced after 1000oC.
Publication Details
Page(s) 282-290
DOI DOI not available
Published Journal: Journal of Chemical Society of Pakistan, Volume: 36, Issue: 2, Year: 2014

Request the full text from PASTIC

0

Citations

0

Downloads

66

Views