Lead Chevrel Phase materials PbMo6S8 have been fabricated in a controlled environment using simple sintering method and a Hot Isostatic method (HIP) operating at pressure up to 2000 atmospheres. The Specific Heat of these materials have been measured using long duration heat pulse method and the A.C. temperature technique. Using the data obtained, the critical temperature Tc, width of the peak ΔT, the jump height, the volumetric averaged upper critical field BC2(T), the Maki’s parameter α, spin-orbit scattering parameter λso, spin-orbit relaxation time τso, and other properties like, the phononic and electronic contributions to specific heat at different temperatures by measuring the Deby Temperature θD and Sommerfeld constant γ, have been studied at large. We found that after HIP, the Tc has been increased about 0.5 K while reducing oxygen contamination during the fabrication process has increased another of 0.5 K in Tc. The slope has been enhanced to about 13% and consequently, BC2(O) has been increased about 65 T, about 20% higher after the HIP process. The HIP process increases the Tc probably because of the improved homogeneity. The higher values of λso>3 leads to screening the effect of paramagnetic limitation by spin-orbit scattering mechanism. The rounded form of the specific heat jump pointed the possibility of the Tc distribution in the sample.