The fiber properties such as fiber length, fineness, tenacity and flexural rigidity have a major influence on the fiber orientation in the rotor-spun yarn. The effect of fiber properties is more obvious in the surface fibers than that of in the core fibers or fibers which form actual yarn body. Physical properties of different fibers are not the same for all the type of fibrous material but depend on the maturity and fineness in the case of cotton and molecular structure and denier of manmade fibers. Five different types of fibers were therefore used to study the effect of fiber properties on the fiber orientation in rotor-spun yarn especially on the surface fibers. Furthermore the surface fibers are randomly wrapped around the yarn body and do not allow the yarn to be untwisted during twist testing. Some of the wrappings produce higher resistance to the untwisting of yarn during twist testing and others are less resistant. The resistance against the untwisting of the yarn depends on the frequency, length of wrappings and the way they are wrapped around the yarn body. This study presents very clear investigation about effect of fibre properties on the frequency, length and types of wrappings. The effect of the number of fibres in the yarn cross-section is also presented. The yarn samples were spun from cotton, trilobal viscose and three types of polyester fibres of different tenacity and linear density. Over all wrapping length and wrapping frequency were analysed with a ’t’ test at 5% probability level by using SPSS (Statistical Package for Social Sciences). It was found that the wrapping frequency increases and over all mean length of wrappings decreases with an increase of number of fibres in the yarn cross-section. Wrapping frequency and tightness of wrappings were higher in the yarns spun from finer polyester than that of the yarns spun from coarser polyester, viscose and cotton.