No Detail Found!

Electrolytic recovery of chromium as chromium salts from tannery waste water. Pakistan

Author(s)
Sirajuddin Center of Excellance in Analytical Chemistry, University of Sindh, Jamshoro, Pakistan
Lutfullah Kakakhel National Centre of Excellence in Physical Chemistry, University of Peshawar, NWFP, Pakistan
Hamid Ali National Centre of Excellence in Physical Chemistry, University of Peshawar, NWFP, Pakistan
Mohammad Abdul-Wasim National Centre of Excellence in Physical Chemistry, University of Peshawar, NWFP, Pakistan
Abstract
Tannery waste water was directly subjected to electrolytic recovery after being diluted to 200 ppm chromium ions containing solution using static sheet electrode system in a simple cell. Chromium was recovered as chromium hydroxide at cathode and as sodium dichromate at anode. Solutions of 1 % H2SO4 or 1 % HNO3 and 1 % NaHCO3 were used for pH adjustment as well as electrolytes. Maximum recovery of 21.5% chromium salts was achieved at pH 3.0 and a cell potential of 0.9V on lead anode and copper cathode in just 15 minutes time of electrolysis.
Publication Details
Page(s) 39-42
DOI DOI not available
Published Journal: Journal of Analytical Chemistry, Volume: 4, Issue: 1, Year: 2003