Beneficiation study of Azad Kashmir graphite ore.

Author(s)
M. A. Bhatti PCSIR Laboratories Complex, Lahore, Pakistan
M. S. Anwar PCSIR Laboratories Complex, Lahore, Pakistan
K. R. Kazmi PCSIR Laboratories Complex, Lahore, Pakistan
A. Amin PCSIR Laboratories Complex, Lahore, Pakistan
R. Mahmood PCSIR Laboratories Complex, Lahore, Pakistan
Abstract
Azad Kashmir graphite ore originally containing 10-14% graphite content was upgraded to more than 85% graphitic carbon with 73% recovery, using froth flotation technique. The pH of the pulp was adjusted with sodium carbonate. Kerosene oil and pine oil were used as collector and frothier respectively. Sodium silicate was employed as depressant. The flotation parameters such as particle size of the feed, pH and % solid of the pulp, speed of impeller, conditioning and flotation time, collecting and frothing agents were optimized to obtain maximum grade and recovery of graphite. The grade of the final concentrate produced is 89.44 % C with particle size of about 74 microns (200 mesh) @ recovery of 72.94%.
Publication Details
Page(s) 36-40
DOI DOI not available
Published Journal: Pakistan journal of scientific research, Volume: 58, Issue: 3--4, Year: 2006

Request the full text from PASTIC

0

Citations

1

Downloads

80

Views