Biodegradation of Polyester Polyurethane Separately by Five Fungi and Three Consortia

Author(s)
Yasir Mustafa University of Science and Technology Bannu,,
Abstract
Human being has prepared multiple plastic items for luxuries and comforts that have occupied a great extent of our habitat. Polyurethane is a polyester type of plastic used in shoes, furniture and foams. Polyester polyurethane is nondegradable and resistance to decomposition. It has led to the environmental pollution like damage to terrestrial ecosystem, aerial ecosystem and aquatic ecosystem. Scientists are looking for the possible solutions to the polyester polyurethane born environmental problems. After thorough review of recycling methods, biodegradation was considered as safe, environment friendly and appropriate mean of polyester polyurethane deterioration. The present work aimed to study the biodegradation of polyester polyurethane separately by five monoculture fungi and three consortia. This study aims to isolate five different types of fungal strains from dumping sites and to test the biodegradation potentials of fungal strains against polyester polyurethane as monocultures (MC) and their three consortia. Moreover to compare the biodegradation efficacy of three consortia of the fungal strains and their monocultures for the efficient biodegradation of polyester polyurethane. The results revealed that the monoculture MCA and MC-E were effective in polyester polyurethane biodegradation in comparison to other monocultures i.e. MC-B, MC-C and MC-D. The degradation of PU by MC-A and MC-E is clearly seen in the pictures and the microscopic images. ATR-FTIR results showed that in the MC-A and MC-E deformation of bonds at wavelength 3320.02 cm-1 is shifted to 3306.72 cm-1 and 3320.48 cm-1 wavelength. MC-E is effective than MC-A follower by MC-B, MC-C and MC-D respectively first, second, third, fourth and fifth in their biodegradation potentials. Moreover Consortium C-1, C8 and C-9 showed biodegradation capacities in the series C-1 followed by C-8 and the C-9. The ATR-FTIR results of C1 and C-8 showed displacement of peak from 3328.02 cm-1 wavelength to 3316.14 cm-1 wavelength, 3304.77 cm-1 wavelength and 3283.62 cm-1 wavelength. The comparision of weight bearing capacities of biodegrading polyester polyurethane indicated that MC-A treated polyester polyurethane bear 0.22 grams, MC-E 0.24 grams, C-1 0.09 grams, C-8 0.08 grams and C-9 0.12 grams. It revealed that among the monoculture fungi MC-A was effective th reducing weight bearing capacity of polyester polyurethane while C-8 was effective among the three consortia. This study will be helpful to recycle polyester polyurethane and no environmental pollution will be caused by polyester polyurethane.
Publication Details
Page(s) 4-5
DOI DOI not available
Published Journal: Abstract Book: 1st International Conference on Recent Advances in Zoology in the Era of Climate Change, May 04-05, 2026, Volume: 1, Issue: 1, Year: 2026

Request the full text from PASTIC

0

Citations

0

Downloads

7

Views