Bismuth based superconducting materials having a general formula Bi2-x Pb0.4Sr2Ca2 Cu3Oy (where x = 0.1, 0.2, 0.3 and 0.4) were synthesized by the simple solid-state reaction method. Each of the samples was initially calcined at three temperatures of 790°C at different heating rates of 2, 5, 10, 14 and 20 °C mm-1 for 24h. The sample pellets were sintered in air at three different temperatures of 835°C for 48 h at the heating rates given above. The lattice parameters (a, b and c) and unit cell volume, Vcell of the samples were calculated by X-ray diffraction (XRD). The dielectrically resistively and ac magnetic susceptibility measurements show that the sample with the value of x = 0.3, sintered at 835°C, at a heating rate of 14°C.min-1 has the highest percentage of the high-Tc (2223) phase, the highest value of Tc(o) =106 K and the lowest room temperature resistivity value.