No Detail Found!

Green synthesis of Cordia myxa incubated ZnO, Fe2O3, and Co3O4 nanoparticle: Characterization, and their response as biological and photocatalytic agent

Author(s)
Sana Batool Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan
Murtaza Hasan Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan; College of Chemistry and Chemical Engineering, Zhongkai University of Agriculture and Engineering, Guangzhou 510225, China
Momina Dilshad Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan
Ayesha Zafar Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan
Tuba Tariq Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan
Ziqian Wu College of Chemistry and Chemical Engineering, Zhongkai University of Agriculture and Engineering, Guangzhou 510225, China
Renxiang Chen College of Chemistry and Chemical Engineering, Zhongkai University of Agriculture and Engineering, Guangzhou 510225, China
Shahbaz Gul Hassan College of Information Technology, Zhongkai University of Agriculture and Engineering, Guangzhou 510225, China
Tauseef Munawar Institute of Physics, IUB, Pakistan
Faisal Iqbal Institute of Physics, IUB, Pakistan
M. Saqib Saif Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan
M. Waqas Department of Biotechnology, The Islamia University of Bahawalpur, Bahawalpur, Pakistan
Xugang Shu College of Chemistry and Chemical Engineering, Zhongkai University of Agriculture and Engineering, Guangzhou 510225, China
Abstract
Imperative necessity for new therapy and catalysts has risen significantly due to infectious agents that are multi-resistant and organic toxins draining into our ecosystem. To address these problems, highly biocompatible Cordia myxa incubated I-ZnO, I-Co3O4, and I-Fe2O3 NPs were prepared and characterized by using a variety of techniques, including ultraviolet–visible spectroscopy (UV–vis), X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR). The XRD diffraction pattern confirmed that I-ZnO hexagonal, while I- Co3O4 and I-Fe2O3 cubic structure. UV–vis spectra show the energy bandgap for I-ZnO, I-Fe2O3, and I-Co3O4 3.35 eV, 2.32 eV, and 2.44 eV, respectively. TEM analyses show the patterns of the morphology of I-ZnO as flower-shaped, I-Fe2O3 as rectangular, I-Co3O4 looks like prism crystals. EDX mapping confirmed the elemental presence of Zn, Fe, Co in the samples. The antibacterial study show that the I-NPs have bigger zone of inhibition (ZOI) than pristine NPs. The highest percentage for E-coli strain obtained in this trend (I- Fe2O3)81%>(I-ZnO)76%>(I-Co3O4)63%. Photocatalytic activity results revealed that the MB dye degraded after 80 min and efficiencies of I-(Fe2O3)98.38 %>I-ZnO98.12%>(I-Co3O4)93.93%. Furthermore, the green synthesis strategy certifies a new pathway for minimizing infections, oxidative stress, and degradation of key pollutants from the environment.
Publication Details
Page(s) 110-110
DOI DOI not available
Published Journal: Abstract Book on Global Science Technology and Management Conference, Volume: 0, Issue: 0, Year: 2023

Request the full text from PASTIC

Keywords
Degradation, Incubated nanoparticle, Cordia Myxa, Microbial inhibition
0

Citations

0

Downloads

262

Views