No Detail Found!

Raw mix designing and clinkerization of high strength Portland cement with Bagasse ash and its impact on clinker moduli and fuel consumption.

Author(s)
Noor-Ul-Amin Institute of Chemical Science, University of Peshawar, Peshawar, Pakistan
Khurshid Ali Institute of Chemical Science, University of Peshawar, Peshawar, Pakistan
Muhammad Tahir Shah National Center of Excellence in Geology, University of Peshawar, Peshawar, Pakistan
Abstract
This paper discusses the utilization of bagasse ash from the sugar mills of North West Frontier Province (NWFP), Pakistan in the raw mix designing for high strength Portland cement; and its impact on clinker moduli and fuel consumption. The resulting clinker and cement was found with in the British and Pakistan standard specifications. 5 % bagasse ash was found as the optimal limit to he blended and pulverized with other raw material prior to clinkerization which saved 6.46 % energy. Among the moduli modulus of alumina (MA), modulus of silica (MS) and lime saturation factor (LSF) were studied. It was found that with 5 % bagasse ash, all the moduli remained with in standards.
Publication Details
Page(s) 370-374
DOI DOI not available
Published Journal: Journal of Chemical Society of Pakistan, Volume: 31, Issue: 3, Year: 2009

Request the full text from PASTIC

0

Citations

0

Downloads

67

Views