No Detail Found!

Comparative study of the flexural strength of maxillary denture bases made in conventional and high impact heat cure acrylic resin

Author(s)
Sadia Akram Abbottabad International Medical & Dental College, Abbottabad, Pakistan; Peshawar Dental College, Peshawar, Pakistan; Khyber Medical University Institute of Dental Sciences, Kohat, Pakistan.
Fahimullah Peshawar Dental College, Peshawar, Pakistan; Khyber Medical University Institute of Dental Sciences, Kohat, Pakistan.
Nuzhat Ayub Peshawar Dental College, Peshawar,Pakistan.
Zudia Riaz Peshawar Dental College,Peshawar,Pakistan
Beenish Haider Peshawar Dental College,Peshawar,Pakistan
Amjad Hanif Peshawar Dental College,Peshawar,Pakistan
Abstract
OBJECTIVE: To compare the flexural strength of maxillary denture bases made in high impact and conventional heat cure acrylic resin. METHODS: This experimental laboratory-based study was conducted in Peshawar Dental College, Materials Research and Centralized Resource Laboratories University of Peshawar, Pakistan. Total 120 edentulous maxillary casts, sixty each of conventional acrylic (30 in subgroup-IA for shallow palate and 30 in subgroup-IB for deep palate and high impact acrylic (30 in subgroup IIA for shallow palate and 30 in subgroup II-B for deep palate) were made. These were then tested for flexural strength using universal testing machine. The load was applied at the rate of 5.0 mm/min. Independent samples t-test was applied for statistical analysis. RESULTS: Mean values of deflection at fracture, fracture load and flexure strength were 0.309±0.059 cm, 87.729±22.497 kg and 13.645± 4.453 kg/cm² respectively. Mean Flexure Strength (kg/cm2) was 8.30±1.27, 16.54±1.77, 10.88±1.01 and 18.85±1 in subgroups I-A, I-B, II-A and II-B respectively (<0.001). Mean deflection at fracture (cm) was 0.24±0.04, 0.29±0.03, 0.35±0.03 & 0.368±0.03 in subgroups I-A, I-B, II-A and II-B respectively (<0.001). Mean Fracture Load kg was 69.97±3.12, 114.9±6.75, 63.28±7.05 and 102.8±5.5 in in subgroups I-A, I-B, II-A and II-B respectively (<0.001). CONCLUSION: High impact acrylic resin was found to have significantly higher flexure strength as compared to conventional acrylic resin.
Publication Details
Page(s) 38-41
Published Journal: Khyber Medical University Journal, Volume: 14, Issue: 1, Year: 2022

Request the full text from PASTIC

Keywords
Palate, Acrylic denture (Non-MeSH), Acrylic Resins (MeSH), Flexural Strength (MeSH), Dental Bases (MeSH), Hard (MeSH), Maxillary (Non-MeSH)
0

Citations

0

Downloads

97

Views