Objective: To compare and evaluate commercial grade composites with novel experimental dental composites. Materials and methods: In this experimental study, two experimental and three commercial composites were tested and compared. The manufacturer data and available literature were used to determine the composition of commercial items. Using a four-figure balance and a concentration kit, we calculated mass and volume changes. Instron testing equipment was used to determine biaxial flexural strength (BFS) and modulus. The push-out test was used to examine composite bonding with dentine using various treatments. Results: Mass change in the distilled water (DW) was 1.3 ± 0.1 %, and in simulated body fluid (SBF) was 1.1 ± 0.1% for all materials. The volume changes in DW were 2.2 ± 0.2 %, and in Simulated body fluid (SBF) was 1.6 ± 0.2 % for all commercial and experimental materials. The BFS declined by 33 % for commercial, and 39 % for experimental materials in 6 months. In the case of modulus, the highest decline was associated with Vertise flow at 49 %, with the least decline of 23 % with commercial bulk filling materials. The push-out force for composites within ivory dentine suggests maximum bond strength with experimental composite C-4META. Conclusion: The experimental composite had the potential to compete with commercial composites in mechanical, chemical, and microscopic properties, without compromising the properties.