No Detail Found!

The comparison of mechanical and thermal properties of carbon nanotubes and graphene naonosheets enhanced phenol-formaldehyde resin.

Author(s)
Xiang-Feng Wu School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuan,China
Yong-Ke Zhao School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuang,China
Yun Zhang School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuang,China
Yu Zhu Wu School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuang,China
Yi Jin Wang School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuang,China
Hui Li Chen Xu Zhang School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuang,China
Xin-Yue Yang School of Materials Science and Engineering, Hebei Provincial Key Laboratory of Traffic Engineering Materials,Shijiazhuang Tiedao University,Shijiazhuang,China
Abstract
Graphene naonosheets were prepared via one-pot hydrothermal process in a Teflon-lined autoclave. Moreover, the mechanical and thermal degradation behaviors of the phenol formaldehyde/carbon nanotubes and phenol formaldehyde/graphene naonosheets composites were discussed. Experimental results showed that the graphene naonosheets possessed better performances than that of carbon nanotubes. When the filler loading was 0.6wt%, tensile strength, Young's modulus, compressive strength and modulus of the as-prepared composites reached their maximum values, which were increased by 77.0, 141.3, 109.1 and 114.8% for graphene naonosheets and 54.7, 85.9, 61.7 and 45.2% for carbon nanotubes than those of pure sample, respectively. In addition, both of these two carbon materials could increase the thermo-stability of the matrix. When their usage amount was 0.6wt%, the thermal degradation temperature (at 10% weight loss) was increased to 255.6°C for phenol formaldehyde/graphene naonosheets composites and 253.5°C for phenol formaldehyde/carbon nanotubes composites from 233.6°C for pure sample.
Publication Details
Page(s) 737-742
DOI DOI not available
Published Journal: Journal of Chemical Society of Pakistan, Volume: 39, Issue: 5, Year: 2017

Request the full text from PASTIC

Keywords
carbon nanotubes, phenol formaldehyde, Graphene naonosheets, thermal degradation