Objectives: To assess compressive strength and effect of duration after photoactivation on the compressive strength of different dual cure bulk fill composites. Methods: Seventy-two disc shaped (4x10mm) specimens were prepared from three dual cure bulk fill materials, ZirconCore (ZC) (n=24), MulticCore Flow (MC) (n=24) and Luxacore Dual (LC) (n=24). Half of the specimens in each material were tested for failure loads after one hour [MC1 (n=12), LC1 (n=12) & ZC1 (n=12)] and the other half in 7 days [MC7 (n=12), LC7 (n=12), ZC7 (n=12)] from photo-polymerization using the universal testing machine at a cross-head speed of 0.5 cm/minutes. Compressive strength was calculated using the formula UCS=4f/πd2. Compressive strengths among different groups were compared using analysis of variance (ANOVA) and Tukey’s multiple comparisons test. Results: Maximum and minimum compressive strengths were observed in ZC7 (344.14±19.22) and LC1 (202.80±15.52) groups. Specimens in LC1 [202.80 (15.52)] showed significantly lower compressive strength as compared to MC1 [287.06 (15.03)] (p