No Detail Found!

Degradation of polyethylene mulching film under different environmental conditions.

Author(s)
Xuemei Zhang School of Chemistry and Chemical Engineering, Shihezi University, Key Laboratory for Chemical Materials of Xinjiang Uygur Autonomous Region, Shihezi, China
Jun Wang Agricultural Techniques Extension Center/Institute of Crops, Xinjiang Agricultural Reclamation Academy of Sciences, Shihezi, China
Baoxun Sui School of Chemistry and Chemical Engineering, Shihezi University, Key Laboratory for Chemical Materials of Xinjiang Uygur Autonomous Region, Shihezi, China
Zicheng Wen School of Chemistry and Chemical Engineering, Shihezi University, Key Laboratory for Chemical Materials of Xinjiang Uygur Autonomous Region, Shihezi, China
Deqiang Li School of Chemistry and Chemical Engineering, Xinxiang University, Xinxiang, China
Zhiyong Li School of Chemistry and Chemical Engineering, Shihezi University, Key Laboratory for Chemical Materials of Xinjiang Uygur Autonomous Region, Shihezi, China
Abstract
To control the degradation of mulching films, polyethylene (PE) films were added with photodegradable additives containing 3.43% (PE-3 film) and 0.44% (PE-4 film) iron stearate. These films were used to assist in cultivating crops under different environmental conditions in Shihezi, Kuitun, and Bole of Xinjiang Province. PE film without any additive was used as a control. Changes in the mechanical and structural properties were observed through tensile strength, elongation at break, and Fourier transform-infrared spectroscopy. Compared with the control PE film, PE-3 and PE-4 films exhibited high-level degradation as carbonyl index increased and viscosity-average molecular weight decreased. Differential scanning calorimetry was used to observe the melting behavior of the PE films with photodegradable additive; crystallinity and melting temperature both slightly increased. The impact of climate conditions on film degradation was investigated. With the same photosensitizer content, film degradation was found to be completed more easily under stronger solar UV radiation and higher relative humidity and temperature (Shihezi, Kuitun, Bole fell in turn). With higher photosensitizer content, the photosensitizer was found to exhibit enhanced degradable effects. Therefore, PE film degradation can be controlled and the requirements of mulching films under different climatic conditions can be achieved by adjusting photosensitizer content.
Publication Details
Page(s) 996-1004
DOI DOI not available
Published Journal: Journal of Chemical Society of Pakistan, Volume: 38, Issue: 5, Year: 2016

Request the full text from PASTIC